Tuesday, April 23, 2013

Re: [MW:17535] Welder Qualification Thickness Limit

sir
    according to ASME Sec IX. for welder qualification maximum  thickness range   is limited ,minimum no problem under  maximum range of qualifcation & wps is guidance  for welder not for limit his qualifcation but welder most be qualified within the essential variable  range(welder perfomance qualification test) of that WPS.
 
Thanks & best regards.
Mohammad Jawed Anwar .
(welding inspector)
Mob no #  +966569799776.


On Tue, Apr 23, 2013 at 1:43 PM, Krish.Saravanan <sarav91@yahoo.com> wrote:
Dear Experts
 
Welder qualification qualified thickness range under ASME Sec IX.
Only maximum qualified weld metal thickness limit given in QW-452.1(b). Is there any minimum thickness limit? Or the minimum thickness is as per WPS which is to be used for production weld? Please advice ….
 Thanks & Regards
Krish
 
 
 
 
 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
 
 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
 
 

No comments:

Re: [MW:34832] Inquiry about Single Bevel with Back Grinding

Dear Uday, As per your question that one is called with backing only,Simple both side you are welding it is backing with strip or without st...