QW 403.9 states that if any weld pass in Single or Multi pass weld exceeds 13 mm (height of each individual pass) then the Base metal thickness beyond  1.1 times the Qualification thickness is an essentail variable that is for any change in Qualification Thickness beyond 1.1 T you need to qualify a new procedure.
 
Normally in SMAW,GTAW, GMAW,FCAW and mostly SAW you don't exceed 13mm of the weld metal thickness for each pass but mostly in Electrogas and Electroslag welding the Thickness exceeds 13 mm.
 
Thanks & Regards

J.Gerald Jayakumar
00968-99438165
From: Maulik Dodiya <maulik.dodiya@gmail.com>
To: materials-welding@googlegroups.com
Sent: Thursday, April 18, 2013 11:03 AM
Subject: [MW:17461] Difficulty in interpretation of ASME sec IX QW403.9

Dear Sirs,
 
I am not getting what exactly ASME Sec IX QW403.9 suggests. Can anybody help me understanding this cluase more deeply.
 
Regards,
Maulik
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
 
 


No comments:

Re: [MW:26937] preheating required for T12 material

Please see below the requirement from ASME Sec.I Power Boilers. I suppose PW-39 exemptions are applicable only for socket welds & seal w...