Welder qualification qualified thickness range under ASME Sec IX.
Only maximum qualified weld metal thickness limit given in QW-452.1(b). Is there any minimum thickness limit? Or the minimum thickness is as per WPS which is to be used for production weld? Please advice ….
 Thanks & Regards
Krish
 
 
 
 
 