Dear Mr Krishnakumar,

 

To standardize the pipe flanges for sizes NPS 26 to NPS 60 for class 75 through to Class 1500 ASME B 16.47 was developed . At that time it was decided to include the flange dimensions as per MSS SP 44 flanges except Class 75 which are ASME/API 605 flanges. Since the dimension of these two classes of flanges were not compatible with each other it was decided that  MSS SP 44 flanges are B 16.47 Series A flanges and  API 605 flanges are designated as B 16.47 Series B flanges.

 

Standards followed:

  • ASME B 16.5 : UP TO SIZE NPS 24
  • ASME B16.47 SR.A / SR.B : UP TO SIZE NPS 60 (for rating150& 300)
  • AWWA C-207 : UP TO SIZE NPS 144 (without Hub) & UP TO SIZE NPS 96 (With Hub) - Pls. refer this standard while giving reference of this for any size.

Other member may offer their comment, 

 Vinod

--- On Fri, 4/29/11, Krishnakumar M S <krishnakumarms01@yahoo.com> wrote:


From: Krishnakumar M S <krishnakumarms01@yahoo.com>
Subject: [MW:10880] Comparison of Large Dia Flanges (B16.47 series A & B) in Refinery services
To: materials-welding@googlegroups.com
Date: Friday, April 29, 2011, 10:46 AM

Hi,

I have to use 30", 42", 48" pipes in Cude Oil, Naphtha, HSD and CRWS services.
What is the criteria between the series A & B for ASME B16.47. Regarding no. of bolts, enonomy, availability etc.
If anyone to know this please.

Regards

Krishnakumar
Fact Engineering & Design Organisation (FEDO)
Cochin, India

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34866] Presentation for WPS ,PQR AND WPQ as per ASME Sec IX in power point

Dear Experts.        If anyone having presentation of WPS,PQR and WPQ  as per ASME  SEC.IX  in power point then please share . Regards Sanja...