Tuesday, April 26, 2011

Re: [MW:10864] acceptance standards for pittings for SA 516 GR 70 Plates

Hi Azmi
 
If it is for new construction, then you can check the minimum thickness, If it doesn't meet your PO or thickness requirement then you can reject the plates, the supplier should have fix the pitting on their side and done all NDE required.
 
Ricardo

On Tue, Apr 26, 2011 at 2:01 AM, Kathalingam Babu <kathalingam.qaqc@ppl.com.sg> wrote:
Hi Azmi,
 
CA-Corrosion Allowance
 
You may refer the material spec. to get the CA.
 
Thanks & Regards,
 
K. Babu
 
----- Original Message -----
From: asad azmi
Sent: Tuesday, April 26, 2011 1:17 PM
Subject: Re: [MW:10852] acceptance standards for pittings for SA 516 GR 70 Plates

Dear mr. Babu,
 
construction code is ASME SEC VIII DIV 1.
 
Pittings were observed  on the plates during material receiving inspection.
 
pls inform me what is CA.
 
thanks and regards

On Tue, Apr 26, 2011 at 4:10 AM, Kathalingam Babu <kathalingam.qaqc@ppl.com.sg> wrote:
Hi Azad,
 
You can consider the CA, as allowable depth of pitting allowed for the respective grade.
 
What is the construction code ?
 
Thanks & Regards,
 
K. Babu
----- Original Message -----
From: asad azmi
Sent: Monday, April 25, 2011 8:06 PM
Subject: [MW:10842] acceptance standards for pittings for SA 516 GR 70 Plates

Dear All,
 
Greetings.
 
what is the acceptance standard for pittings on SA 516 GR 70 Plate.
 
I mean what is the depth and diameter allowed.
 
Thanks and Regards
 
Asad Azmi

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34866] Presentation for WPS ,PQR AND WPQ as per ASME Sec IX in power point

Dear Experts.        If anyone having presentation of WPS,PQR and WPQ  as per ASME  SEC.IX  in power point then please share . Regards Sanja...