Tuesday, April 26, 2011

Re: [MW:10856] ASME/ASTM equivalent of S355J2+N

ABS Grade EH36
Also, ASTM A131 Gr.EH36
 
Thanks & Regards,
 
K. Babu
----- Original Message -----
Sent: Tuesday, April 26, 2011 4:09 PM
Subject: [MW:10855] ASME/ASTM equivalent of S355J2+N

Dear All

What is the ASTM/ASME equivalent of structural material S355J2+N (minimum yield strength 355 MPa, Tensile 470 to 630 MPa, C: 0.20 max, Si: 0.55 max, Mn: 1.60 max , CE: 0.45 max). A link to reference document stating the same would be much appreciated.

Thanks & best regards

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34916] Applicability of Impact requirement as per ASME B31.3

Dear All, Design code – ASME B31.3, Welding Code- ASME BPVC SEC IX Material  to be used used during Fabrication - SA 333Gr6 (P No.1 G...