On Sat, Apr 23, 2011 at 7:30 PM, praveen nair <praveen_nair9894@yahoo.co.in> wrote:
dear experts

we have aproject on inconel 600 . in that we want to weld inconel600 to ss304 and ms. can i use inco weld 82 as filler wire for both in tig.inconel of 16mm thick

praveen nair

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:34874] ASME IX, groove weld during WQT limits for Fillet Weld production

Hi David,  There are two points in WQT. 1. Thickness of Base Metal -T 2. Thickness of Weld Metal -t When you use a combination of two proces...