Sunday, April 24, 2011

Re: [MW:10816] ASME sect IX PQR thick Qualified

Hi,
 
No, The qualified thickness range will be 5mm to 30mm (If impact test is not required).
 
If you want to weld a 3mm thk, you have to qualify @ thk of less than or equal to 10mm.
 
Cheers!
 
Raj

On Sat, Apr 23, 2011 at 11:33 AM, Zakaria ghrab <zakaria.ghrab@gmail.com> wrote:
Hi all,

  We have a PQR, 15 mm Thickness, welded 6mm GTAW, 9mm SMAW.
According ASME sect IX, table QW-451.1, the Qualified Thickness "T" of base metal qualified will be 1.5 mm to 30 mm and the deposit weld thikness GTAW will be 12 mm max "2xt".
 Means if i have to weld pipe thick 3 mm i can't use this PQR, i'm right ?

--
زكرياء غراب


--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:34832] Inquiry about Single Bevel with Back Grinding

Dear Uday, As per your question that one is called with backing only,Simple both side you are welding it is backing with strip or without st...