[MW:10834] MW: 10828- Hastelloy C22 welding to SA516-70N welding

Hello Vijay,
 
The recomended welding consumable is  SFA 5.11-E-NiCrMo-10(SMAW) or SFA 5.14-ERNiCrMo-10 (GTAW/GMAW). You may choose any one of the above processes depending on the joint details, thickness and other aspects involved.
 
Are there  other requirements for welding qualification , e.g corrosion or other requirements  over and above ASME -Sec-IX requirements.If so please take special notes.
 
Thanks.
 
Pradip Goswami,P.Eng.IWE
Welding & Metallurgical Specialist & Consultant
Ontario,Canada.
Email-pgoswami@sympatico.ca,
 


From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of vijay
Sent: Sunday, April 24, 2011 9:26 PM
To: weldinggang@googlegroups.com; materials-welding@googlegroups.com
Subject: [MW:10828] Hastelloy C22 welding to SA516-70N welding

Dear Friends,

Please advice for the welding process, filler material/consumable and other requirement for the below situation:
Hastelloy C22 to SA516-70N for Heat-exchanger Wearplate to Support Rib Fillet weld

Regards,
Vijay

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:34874] ASME IX, groove weld during WQT limits for Fillet Weld production

Hi David,  There are two points in WQT. 1. Thickness of Base Metal -T 2. Thickness of Weld Metal -t When you use a combination of two proces...