Hi,

A 358 is specifies about variations in dimensions as mentioned below.
Refer 7.1.3 ??

7. Permissible Variations in Dimensions
7.1 Permissible Variations—The dimensions at any point in a length of
pipe shall not exceed the following:
7.1.1 Outside Diameter—Based on circumferential measurement, 60.5 % of
the specified outside diameter.
7.1.2 Out-of-Roundness—Difference between major and minor outside
diameters, 1 %.
7.1.3 Alignment—Using a 10-ft or 3-m straightedge placed so that both
ends are in contact with the pipe, 1⁄8in. [3 mm].
7.1.4 Thickness—The minimum wall thickness at any point in the pipe
shall not be more than 0.01 in. [0.3 mm] under the nominal thickness.

Other code A530 (Standard Specification for General Requirements for
Specialized Carbon and Alloy Steel Pipe) is specifies "Straightness
Tolerances" and mentioned in table-3. (But this is not applicable for
your case) - For your info only.

I just want to throw some light on your query !!!

Cheers!

Raj


On Apr 21, 3:30 pm, biju <biju....@gmail.com> wrote:
> Hi,
>
> We received some stainless steel pipes A358TP316L 16"SCH-10S having an
> out of straightness 23 to 25 mm .Pipe length is around
> 11.800mtrs.Client rejected those pipes.Is B31.3 saying any thing about
> out of straightness requirements. If their please provide me the
> details. Also is their any manufacturing spec requirements for this?
>
> regards,
>
> Biju

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34866] Presentation for WPS ,PQR AND WPQ as per ASME Sec IX in power point

Dear Experts.        If anyone having presentation of WPS,PQR and WPQ  as per ASME  SEC.IX  in power point then please share . Regards Sanja...