Monday, February 29, 2016
[MW:24414] Repair local PWHT,360band local PWHT,full furness PWHT.
PIPING Mat is cs and 35mm WPS is qualifed with dull furness pwht.welding process SMAW AND GTAW.code is ASMEix and 31.3.
To improve productivity and avoid full furness PWHT for only repair joints
WHAT EXTRA THINGS OR NDE OR PRECAUTION SHOULD TAKE FOR LOCAL REAPIR PWHT OR 360 BAND PWHT?
Is it allowed normally or you will have to have WPS.?
--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/4459d65b-4b0e-4955-ac40-88024ed3919b%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.
[MW:24415] PWHT
Dear all,
I have two queries:
MOC: P8Gr1(SS347 internal)
PWHT on job with LAS is at 705+/-10 degree C for 10 hrs.
Available PQR: 700 degree C for 8 hrs.
Can I support same PQR for welding of SS347 internal which will undergo PWHT at 705+/- 10 degree C along with LAS???
Impact: not applicable for SS.
Second query:
Interpretation of QW407.1 (b).
Regards,
Maulik
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAFK0MUMCrJL9dRmq0Q%3DDEJpfNmP%3DJ%3DRmrTk4fzV7cjfUj7FKdw%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.
Re: [MW:24411] Fillet weld cracks below 6 mm with suitable NDT.
Dear Sir,
You may carryout with UT and sketch is attached
Thanking You.
With Warm Regards,
Muthu Barathi P.
Mobile : +919967300544 (Only message )
Mobile No. +965 50989210 (KUWAIT) after 8PM
From: Mohammed Ghani <ghani386@gmail.com>
Sent: Sun, 28 Feb 2016 16:17:38
To: materials-welding@googlegroups.com
Subject: [MW:24396] Fillet weld cracks below 6 mm with suitable NDT.
Dear experts,
I want to locate Fillet weld cracks below 6 mm for 22 mm plate with double V preparation.
Is there any special techniques from NDT I can use to identify cracks below 6 mm.
Please suggest me if any suitable NDT procedure for this. It is a bit urgent.
Appreciate your respond.
Regards,
Mohammed ghani.
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAG7AWVhBp4jWOun%3DrCPmJuh%2B1PLib%3D9%2BFM4KWDSsuRAUVRSVsg%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.
Get your own FREE website, FREE domain & FREE mobile app with Company email. | Know More > |
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/1456656458.S.8693.1535.f5-224-126.1456741228.22099%40webmail.rediffmail.com.
For more options, visit https://groups.google.com/d/optout.
[MW:24411] RE: Material Certificate & test requirements
Dear experts,
I need to procure this material
Hex Bolt & 2 nuts M20 x 75 based on ISO 3506-1 / A4-80 based on your experience, could you give me your feedback about material certificate, tests requirements and which I need to work with.
Thanks
ludmila
Re: [MW:24409] Welding by SAW process is it mandatory for heavy thick vessels in H2 service
From: Kannayeram Gnanapandithan <kgpandithan@gmail.com>
Sent: Mon, 29 Feb 2016 11:10:12
To: materials-welding <materials-welding@googlegroups.com>
Subject: Re: [MW:24404] Welding by SAW process is it mandatory for heavy thick vessels in H2 service
--Almost 20 years ago I was in a tank farm project were field welds were performed by means of sawSent from my BlackBerry 10 smartphone.
From: PrasadSent: Σάββατο, 27 Φεβρουαρίου 2016 - 09:02To: Materials & WeldingReply To: materials-welding@googlegroups.comSubject: [MW:24384] Welding by SAW process is it mandatory for heavy thick vessels in H2 serviceDear welding experts,--We are manufacturing heavy wall vessels for H2 service.MOC SA 516 Gr 70. Thick 56 mmDue to large size vessels are to be supplied in two sections.Hence on site weld joint will have to be done at place of installation.At shop we are using SAW process for welding.At field rotating is not possible and we want to use SMAW process.Our client is asking us to use SAW process for field weld joint also.We know that SAW is semi automatic & more productive process.My question is whether is their any restriction to use SMAW process.Request experts to give their valuable views to convience client technically.Best regards,Prasad Ghanekar
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/bb19d5b1-6c54-45fe-8e91-1346dd8c9617%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/20160227154234.6713426.85120.1966%40gmail.com.
For more options, visit https://groups.google.com/d/optout.
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAJzm4eMGZGYtAK5gG1pnsB4W2OZ9KngLfpg5Mn4_MM1Nib1tGQ%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.
Get your own FREE website, FREE domain & FREE mobile app with Company email. | Know More > |
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/1456724412.S.18199.30999.f6-235-206.1456734926.27074%40webmail.rediffmail.com.
For more options, visit https://groups.google.com/d/optout.
Re: [MW:24409] Welding by SAW process is it mandatory for heavy thick vessels in H2 service
From: Kannayeram Gnanapandithan <kgpandithan@gmail.com>
To: materials-welding <materials-welding@googlegroups.com>
Sent: Monday, 29 February 2016 6:31 AM
Subject: Re: [MW:24404] Welding by SAW process is it mandatory for heavy thick vessels in H2 service
--Almost 20 years ago I was in a tank farm project were field welds were performed by means of sawSent from my BlackBerry 10 smartphone.
From: PrasadSent: Σάββατο, 27 Φεβρουαρίου 2016 - 09:02To: Materials & WeldingReply To: materials-welding@googlegroups.comSubject: [MW:24384] Welding by SAW process is it mandatory for heavy thick vessels in H2 serviceDear welding experts,--We are manufacturing heavy wall vessels for H2 service.MOC SA 516 Gr 70. Thick 56 mmDue to large size vessels are to be supplied in two sections.Hence on site weld joint will have to be done at place of installation.At shop we are using SAW process for welding.At field rotating is not possible and we want to use SMAW process.Our client is asking us to use SAW process for field weld joint also.We know that SAW is semi automatic & more productive process.My question is whether is their any restriction to use SMAW process.Request experts to give their valuable views to convience client technically.Best regards,Prasad Ghanekar
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/bb19d5b1-6c54-45fe-8e91-1346dd8c9617%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/20160227154234.6713426.85120.1966%40gmail.com.
For more options, visit https://groups.google.com/d/optout.
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAJzm4eMGZGYtAK5gG1pnsB4W2OZ9KngLfpg5Mn4_MM1Nib1tGQ%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.
RE: [MW:24407] Fillet weld cracks below 6 mm with suitable NDT.
After performing gauging, we found most of the cracks are below 6mm
How u know crack is exactly 6mm below??
quite interesting.
Do RT.
--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/1346669f-f39d-4460-a282-dc42b4377911%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAG7AWVjhGLOwWX-UqX7t3YWCO8GLEZKuiFzVcP9OHk3-Ld9VCw%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.
Re: [MW:24407] Fillet weld cracks below 6 mm with suitable NDT.
Dear,
It is fillet weld for sure. ...
Regards,
Mohammed ghani.
Hello Sir,I hope it is Butt weld T-Joint, so you can apply normal UT also.RegardsJayachandran V.--On Sun, Feb 28, 2016 at 1:01 PM, Mohammed Ghani <ghani386@gmail.com> wrote:Dear experts,
I want to locate Fillet weld cracks below 6 mm for 22 mm plate with double V preparation.
Is there any special techniques from NDT I can use to identify cracks below 6 mm.Please suggest me if any suitable NDT procedure for this. It is a bit urgent.
Appreciate your respond.
Regards,
--
Mohammed ghani.
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAG7AWVhBp4jWOun%3DrCPmJuh%2B1PLib%3D9%2BFM4KWDSsuRAUVRSVsg%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CANvSE6m_tZVX3%2B5-u-jbGYDg0D%2BHmeuTQpJUARQ3qzrMVf_cZg%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAG7AWVjeWavS6mrZVTGQ3bdQ2%2BdtNGGHeJ6nPHz8Q%3DCKRi0%2BjQ%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.
Re: [MW:24406] Fillet weld cracks below 6 mm with suitable NDT.
From: Mohammed Ghani Sent: Δευτέρα, 29 Φεβρουαρίου 2016 - 05:19 To: materials-welding@googlegroups.com Reply To: materials-welding@googlegroups.com Subject: RE: [MW:24403] Fillet weld cracks below 6 mm with suitable NDT. |
Dear,
Thanks for the reply.
This is for RIG spudcan crack found after 3 years in service. .. I need to rectify if any more possible cracks available in fillet joints... usually with MPI we could locate cracks upto 5 to 6 mm...
Please prove me more suggestions.
Regards,
Mohammed ghani.
--Hello
I recomend Phased Array ultrasonic technic.
Agustín
Level 2 VT PT MT UT RT
Enviado desde mi smartphone Samsung Galaxy.
-------- Mensaje original --------
De: Mohammed Ghani <ghani386@gmail.com>
Fecha:28/02/2016 04:31 AM (GMT-04:30)
Para: materials-welding@googlegroups.com
Cc:
Asunto: [MW:24396] Fillet weld cracks below 6 mm with suitable NDT.Dear experts,
I want to locate Fillet weld cracks below 6 mm for 22 mm plate with double V preparation.
Is there any special techniques from NDT I can use to identify cracks below 6 mm.Please suggest me if any suitable NDT procedure for this. It is a bit urgent.
Appreciate your respond.
Regards,
--
Mohammed ghani.
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAG7AWVhBp4jWOun%3DrCPmJuh%2B1PLib%3D9%2BFM4KWDSsuRAUVRSVsg%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/h8u94emwh70urwdu19wnl0ig.1456666226993%40email.android.com.
For more options, visit https://groups.google.com/d/optout.
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAG7AWVhUaR90G2HdKQb8uuSxE5Ne_WhFkS0RksZdiMUwZ%2BWojw%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.
Re: [MW:24405] RE: 24355] Impact Test & cooling Rate-Preheating (carbon steel)
--One more addition to Alan's good comment:In case of lower thicknesses, the cooling rate tends to increase and may lead to martensite formation. But it is not so slow and sustained a cooling rate as to promote grain growth/reduced ductility, as you are allowed to weld between preheat & interpass temperatures.BR,Shashank C Vagal
From: Alan Denney <alan@denney1.freeserve.co.uk>
To: materials-welding@googlegroups.com
Sent: Tuesday, 23 February 2016 2:59 AM
Subject: [MW:24358] RE: 24355] Impact Test & cooling Rate-Preheating (carbon steel)
Alan DenneyAKD Materials Consulting LtdFrom: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Mohd Siraj
Sent: 22 February 2016 09:22
To: Materials & Welding <materials-welding@googlegroups.com>
Subject: [MW:24355] Impact Test & cooling Rate-Preheating (carbon steel)Dear all,Background:impact testing is more critical for less(low)thickness than higher thickness.Reason :fine grain form during fast cooling and course grain form during slow cooling.Question is:Preheating use to lower the cooling rate for higher thickness.So lower the cooling rate means form the course grain,course grain lower the toughness.Preheating contributing to lower the toughness?--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/3247d39d-f53a-4bc4-aee8-79f73a1d95d8%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.This email has been scanned by BullGuard antivirus protection.For more info visit www.bullguard.com--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/003801d16db8%2430d2dab0%2492789010%24%40denney1.freeserve.co.uk.
For more options, visit https://groups.google.com/d/optout.
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/613526275.231430.1456591879950.JavaMail.yahoo%40mail.yahoo.com.
For more options, visit https://groups.google.com/d/optout.
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAJzm4eM9fdE1Yu4c9%3D0bV7xkqtuHBhCK2FMMPsDbbrwhwVt17g%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.
Re: [MW:24404] Welding by SAW process is it mandatory for heavy thick vessels in H2 service
--Almost 20 years ago I was in a tank farm project were field welds were performed by means of sawSent from my BlackBerry 10 smartphone.
From: PrasadSent: Σάββατο, 27 Φεβρουαρίου 2016 - 09:02To: Materials & WeldingReply To: materials-welding@googlegroups.comSubject: [MW:24384] Welding by SAW process is it mandatory for heavy thick vessels in H2 serviceDear welding experts,--We are manufacturing heavy wall vessels for H2 service.MOC SA 516 Gr 70. Thick 56 mmDue to large size vessels are to be supplied in two sections.Hence on site weld joint will have to be done at place of installation.At shop we are using SAW process for welding.At field rotating is not possible and we want to use SMAW process.Our client is asking us to use SAW process for field weld joint also.We know that SAW is semi automatic & more productive process.My question is whether is their any restriction to use SMAW process.Request experts to give their valuable views to convience client technically.Best regards,Prasad Ghanekar
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/bb19d5b1-6c54-45fe-8e91-1346dd8c9617%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/20160227154234.6713426.85120.1966%40gmail.com.
For more options, visit https://groups.google.com/d/optout.
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAJzm4eMGZGYtAK5gG1pnsB4W2OZ9KngLfpg5Mn4_MM1Nib1tGQ%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.
Re: [MW:24401] Fillet weld cracks below 6 mm with suitable NDT.
Dear experts,
I want to locate Fillet weld cracks below 6 mm for 22 mm plate with double V preparation.
Is there any special techniques from NDT I can use to identify cracks below 6 mm.Please suggest me if any suitable NDT procedure for this. It is a bit urgent.
Appreciate your respond.
Regards,
--
Mohammed ghani.
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAG7AWVhBp4jWOun%3DrCPmJuh%2B1PLib%3D9%2BFM4KWDSsuRAUVRSVsg%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CANvSE6m_tZVX3%2B5-u-jbGYDg0D%2BHmeuTQpJUARQ3qzrMVf_cZg%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.
Sunday, February 28, 2016
RE: [MW:24401] Fillet weld cracks below 6 mm with suitable NDT.
quite interesting.
Do RT.
--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/1346669f-f39d-4460-a282-dc42b4377911%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.
RE: [MW:24403] Fillet weld cracks below 6 mm with suitable NDT.
Dear,
Thanks for the reply.
This is for RIG spudcan crack found after 3 years in service. .. I need to rectify if any more possible cracks available in fillet joints... usually with MPI we could locate cracks upto 5 to 6 mm...
Please prove me more suggestions.
Regards,
Mohammed ghani.
--Hello
I recomend Phased Array ultrasonic technic.
Agustín
Level 2 VT PT MT UT RT
Enviado desde mi smartphone Samsung Galaxy.
-------- Mensaje original --------
De: Mohammed Ghani <ghani386@gmail.com>
Fecha:28/02/2016 04:31 AM (GMT-04:30)
Para: materials-welding@googlegroups.com
Cc:
Asunto: [MW:24396] Fillet weld cracks below 6 mm with suitable NDT.Dear experts,
I want to locate Fillet weld cracks below 6 mm for 22 mm plate with double V preparation.
Is there any special techniques from NDT I can use to identify cracks below 6 mm.Please suggest me if any suitable NDT procedure for this. It is a bit urgent.
Appreciate your respond.
Regards,
--
Mohammed ghani.
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAG7AWVhBp4jWOun%3DrCPmJuh%2B1PLib%3D9%2BFM4KWDSsuRAUVRSVsg%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/h8u94emwh70urwdu19wnl0ig.1456666226993%40email.android.com.
For more options, visit https://groups.google.com/d/optout.
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAG7AWVhUaR90G2HdKQb8uuSxE5Ne_WhFkS0RksZdiMUwZ%2BWojw%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.
RE: [MW:24399] REPAIR OF METAL LOSS BY COLD WELD (BELZONA)
-----Original Message-----
From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Mohd Siraj
Sent: Sunday, February 28, 2016 1:56 AM
To: Materials & Welding <materials-welding@googlegroups.com>
Subject: Re: [MW:24397] REPAIR OF METAL LOSS BY COLD WELD (BELZONA)
As per API570 &510,
Reapir depend on thickness measurement.
permenant repair shall be done by flushing plate welding/hollow cylinder.
Temporary leak can b arrested by leak clamp.
--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/8a835f29-6b91-44ca-b687-c88c59358831%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.
--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/BAY403-EAS55379CB4ACF43EB22912A0DBB90%40phx.gbl.
For more options, visit https://groups.google.com/d/optout.
RE: [MW:24399] Fillet weld cracks below 6 mm with suitable NDT.
I recomend Phased Array ultrasonic technic.
Agustín
Level 2 VT PT MT UT RT
Enviado desde mi smartphone Samsung Galaxy.
-------- Mensaje original --------
De: Mohammed Ghani <ghani386@gmail.com>
Fecha:28/02/2016 04:31 AM (GMT-04:30)
Para: materials-welding@googlegroups.com
Cc:
Asunto: [MW:24396] Fillet weld cracks below 6 mm with suitable NDT.
Dear experts,
I want to locate Fillet weld cracks below 6 mm for 22 mm plate with double V preparation.
Is there any special techniques from NDT I can use to identify cracks below 6 mm.
Please suggest me if any suitable NDT procedure for this. It is a bit urgent.
Appreciate your respond.
Regards,
Mohammed ghani.
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAG7AWVhBp4jWOun%3DrCPmJuh%2B1PLib%3D9%2BFM4KWDSsuRAUVRSVsg%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.
[MW:24396] Fillet weld cracks below 6 mm with suitable NDT.
Dear experts,
I want to locate Fillet weld cracks below 6 mm for 22 mm plate with double V preparation.
Is there any special techniques from NDT I can use to identify cracks below 6 mm.
Please suggest me if any suitable NDT procedure for this. It is a bit urgent.
Appreciate your respond.
Regards,
Mohammed ghani.
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAG7AWVhBp4jWOun%3DrCPmJuh%2B1PLib%3D9%2BFM4KWDSsuRAUVRSVsg%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.
Re: [MW:24397] REPAIR OF METAL LOSS BY COLD WELD (BELZONA)
Reapir depend on thickness measurement.
permenant repair shall be done by flushing plate welding/hollow cylinder.
Temporary leak can b arrested by leak clamp.
--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/8a835f29-6b91-44ca-b687-c88c59358831%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.
Re: [MW:24397] Welding by SAW process is it mandatory for heavy thick vessels in H2 service
Dear,
You can use any welding procedures at site as per difficulties, subjected you shall provide an approved WPS/PQR for that thickness limit..
Regards,
Mohammed.On 27 Feb 2016 10:02, "Prasad" <prsgne@gmail.com> wrote:--Dear welding experts,--We are manufacturing heavy wall vessels for H2 service.MOC SA 516 Gr 70. Thick 56 mmDue to large size vessels are to be supplied in two sections.Hence on site weld joint will have to be done at place of installation.At shop we are using SAW process for welding.At field rotating is not possible and we want to use SMAW process.Our client is asking us to use SAW process for field weld joint also.We know that SAW is semi automatic & more productive process.My question is whether is their any restriction to use SMAW process.Request experts to give their valuable views to convience client technically.Best regards,Prasad Ghanekar
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/bb19d5b1-6c54-45fe-8e91-1346dd8c9617%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAG7AWVidRd4PZxs%2B25s%2B_uKGftiGTeKfqoEidSica8Qo1_XNEA%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAOUP4qJRACncGxSgLNcYk3dELQ8u7KgwhMdchZQgOstCYBYbPA%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.
Re: [MW:24394] Welding by SAW process is it mandatory for heavy thick vessels in H2 service
Dear,
You can use any welding procedures at site as per difficulties, subjected you shall provide an approved WPS/PQR for that thickness limit..
Regards,
Mohammed.
Dear welding experts,--We are manufacturing heavy wall vessels for H2 service.MOC SA 516 Gr 70. Thick 56 mmDue to large size vessels are to be supplied in two sections.Hence on site weld joint will have to be done at place of installation.At shop we are using SAW process for welding.At field rotating is not possible and we want to use SMAW process.Our client is asking us to use SAW process for field weld joint also.We know that SAW is semi automatic & more productive process.My question is whether is their any restriction to use SMAW process.Request experts to give their valuable views to convience client technically.Best regards,Prasad Ghanekar
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/bb19d5b1-6c54-45fe-8e91-1346dd8c9617%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAG7AWVidRd4PZxs%2B25s%2B_uKGftiGTeKfqoEidSica8Qo1_XNEA%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.
Re: [MW:24395] RE: 24355] Impact Test & cooling Rate-Preheating (carbon steel)
--One more addition to Alan's good comment:In case of lower thicknesses, the cooling rate tends to increase and may lead to martensite formation. But it is not so slow and sustained a cooling rate as to promote grain growth/reduced ductility, as you are allowed to weld between preheat & interpass temperatures.BR,Shashank C Vagal
From: Alan Denney <alan@denney1.freeserve.co.uk>
To: materials-welding@googlegroups.com
Sent: Tuesday, 23 February 2016 2:59 AM
Subject: [MW:24358] RE: 24355] Impact Test & cooling Rate-Preheating (carbon steel)
Alan DenneyAKD Materials Consulting LtdFrom: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Mohd Siraj
Sent: 22 February 2016 09:22
To: Materials & Welding <materials-welding@googlegroups.com>
Subject: [MW:24355] Impact Test & cooling Rate-Preheating (carbon steel)Dear all,Background:impact testing is more critical for less(low)thickness than higher thickness.Reason :fine grain form during fast cooling and course grain form during slow cooling.Question is:Preheating use to lower the cooling rate for higher thickness.So lower the cooling rate means form the course grain,course grain lower the toughness.Preheating contributing to lower the toughness?--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/3247d39d-f53a-4bc4-aee8-79f73a1d95d8%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.This email has been scanned by BullGuard antivirus protection.For more info visit www.bullguard.com--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/003801d16db8%2430d2dab0%2492789010%24%40denney1.freeserve.co.uk.
For more options, visit https://groups.google.com/d/optout.
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/613526275.231430.1456591879950.JavaMail.yahoo%40mail.yahoo.com.
For more options, visit https://groups.google.com/d/optout.
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAEagfUjzRAMRCjnwLRZ8N9CahUzM7JBg_5dz2%3DF9ZM%2Bz8Kb%2BkA%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.
[MW:34916] Applicability of Impact requirement as per ASME B31.3
Dear All, Design code – ASME B31.3, Welding Code- ASME BPVC SEC IX Material to be used used during Fabrication - SA 333Gr6 (P No.1 G...
-
Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? ...
-
Definition of buttering from ASME Section IX, QW/QB-492 Definitions: Buttering: the addition of material, by welding, on one or bot...
-
Section I. PRINT READING 3-1. GENERAL a. Drawings . Drawing or sketching is a universal language used to convey all necessary information to...