Fabricator feels that as 10ISO16 wire is seen in both the films, will we miss a defect more than this size in D4. As you have suggested we are consulting the designer and working out options without repair.

Regards

Mohan

On Sat, 20 Apr 2013 01:08:26 -0700 (PDT), SV Swamy wrote
> If I remember right D2 is a slower finer grained film. Thus it may show some fine indications missed by D4. You can switch to D2 but you may find such indications and would have a problem deciding whether to leave them alone (and monitor them later in service if possible) or repair them. Repair may sometimes worsen and introduce more discontinuities. 
>
> Better discuss with designer if possible before switching. 
>
> Swamy
> Retd. QA Metallurgist
> Nuclear Fuel Complex, Hyderabad
>
> On Friday, April 19, 2013 12:10:35 PM UTC+5:30, Mohanananthanarayanan KR wrote:
Dear all,
>
> As per specification we have D4 film to be used for radiography of 7.8mm welds
> of M250.As an investigation of a defect in UT D2 film was used and it detected
> faint indications. The sensitivity IQI is seen in both the films as per
> specification. Should we change to D2 film?
>
> Regards
>
> Ananthanarayanan
> Trivandrum
>
> **Print this e-mail only if absolutely necessary. Save paper and keep India Green**
>
> ***The information contained in this e-mail message and / or attachments to it may contain confidential or privileged information. If you are not the intended recipient and received this e-mail in error, please notify us by reply e-mail / telephone and  delete the message and attachments permanently. Thank you.***
>
>

> --
> To post to this group, send email to materials-welding@googlegroups.com
> To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
> For more options, visit this group's bolg at http://materials-welding.blogspot.com/
> http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
>  
> The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
> ---
> You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
> To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
> For more options, visit https://groups.google.com/groups/opt_out.
>  
>  


No comments:

[MW:34866] Presentation for WPS ,PQR AND WPQ as per ASME Sec IX in power point

Dear Experts.        If anyone having presentation of WPS,PQR and WPQ  as per ASME  SEC.IX  in power point then please share . Regards Sanja...