Saturday, April 20, 2013

Re: [MW:17486] IBR piping


Hi there,
Any piping dat has the pressure > 3.5 kg/cm2 or sizing more than 10" ID and is connected to the steam generating circuit comes under IBR.

All such piping shall have IBR test certificate I.e form 3c or 3d..

And for closed vessel exceeding 22.5 ltrs in capacity and used for generating steam under pressure cmes under IBR.

If ur equipment is IBR then its components also comes under the regulation.

Also Kindly refer the drawing as design code will be mentioned in it. If its IBR then dat will also be mentioned.

Hope this reply helps..

Regards,
Nishant

Sent from Yahoo! Mail..



From: Pradip Ghosh <pradipg2@gmail.com>;
To: <materials-welding@googlegroups.com>;
Subject: [MW:17477] IBR piping
Sent: Sat, Apr 20, 2013 10:14:17 AM

Dear expert,

How can I define IBR and non IBR piping ? I have steam heating coil piping inside tank, is it comes under IBR ?


Pradip Ghosh


--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
 
 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
 
 

No comments:

[MW:34866] Presentation for WPS ,PQR AND WPQ as per ASME Sec IX in power point

Dear Experts.        If anyone having presentation of WPS,PQR and WPQ  as per ASME  SEC.IX  in power point then please share . Regards Sanja...