I think 404.10 is for SAW process, here is the case of SMAW process.
E 7018 can not replace E 7018-1, as there is no weld metal chemistry defined in Sec II C for E 7018-1, also there is no F No. for E 7018-1 as per section IX.On Wed, Apr 17, 2013 at 4:18 PM, Chauhan Hemal <hemal_mech1@yahoo.co.in> wrote:
Dear binu,For more information kindly read QW-404.10,ASME SEC-9,Page no:65 for your reference.....Regards,hemal chauhanEngineers india limited.
From: Mhaskar Aly <mhaskar.aly@gmail.com>
To: materials-welding@googlegroups.com
Sent: Tuesday, 16 April 2013 4:25 PM
Subject: Re: [MW:17438] E 7018 used instead of E7018-1
--DearQualify Welding procedure with E7018 and carry out tensile, bend & impact testing...if all tests are OK you can convince your Client those weld joints are meeting requirement of impact properties.....AliOn Sun, Apr 14, 2013 at 2:11 PM, Binu Nair <binugnair1984@gmail.com> wrote:
Dear Experts,Our welders are used E7018 instead of 7018-1 for A333 Gr-6.Now client is asking to cut the joints.Moreover they are asking to prove the remaining joints whether they are welded with 7018-1 or not.Can anybody suggest a suitable method such as any NDT to prove that ?So please send your valuable suggestion with reference to code.Thanks & regards,Binu.--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
No comments:
Post a Comment