This is quite common specially with equipment
After welding as per ASME xiii RT shall be carried out on the weldolet welding as well as two additional shots 3 inches either side of the weldolet welded
I hope this helps
Sent from my iPhone
Regards B. Alavi
--Dear Experts ,Weldolet ( Drain point ) is overlapping Long seam of 48 inch 90 deg LR Elbow ..Design pressure : 96 BarDesign temp ( Max/Min) : 80/5 deg CHydrotest Pressure : 120 BarNDT : 100 % RT , MPIApplication : SubseaService: Offshore Non Sour, Non Corrosive , HC Crude Blended OilSpec : ASME B 31.4Elbow Spec: ASTM A 860 WPHY 65 WLDDKindly refer attached snap ..My Question is what should be the NDT to be performed before & after welding of weldolet ? please put code/client reference .. ( Any )( Kindly let me know if more information is required)Thanks & regards.ABHISHEK GHOSH
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
<IMG_0879.JPG>
No comments:
Post a Comment