Dear sumod,

 

If a WPS have GTAW+ SMAW , then each process can be used individually with in all essential variables (QW 200.4.a). So obviously you can make individual WPS from combined PQR

 

 

 

S.Binoy

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of sumod s
Sent: Tuesday, April 16, 2013 1:16 PM
To: materials-welding@googlegroups.com
Subject: [MW:17440] Invidual WPS from combined PQR

 

Dear,

 

I have a PQR for GTAW +SMAW. Can i make seperate WPS for GTAW and SMAW(with backing) from this PQR. (with in all limits of thickness)

 

Sumod

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
 
 

No comments:

[MW:34919] Welder qualification certificate

Dear All     anyone can share a format for welder certificate and card format        Thanks & Best Regards Saleem manhappulath Mob:+9665...