Wednesday, April 17, 2013

RE: [MW:17444] Re: 17357] Austinitic Stainless steel piping, corrosion environnement

I work with cooling water system on refinery, but we use cement line and is cheapest.
Regards
 
Carlos Oliveros
Welding Inspector
Colombian/Venezuelan
 

Date: Sat, 13 Apr 2013 07:12:31 +0000
Subject: [MW:17368] Re: 17357] Austinitic Stainless steel piping, corrosion environnement
From: zakaria.ghrab@gmail.com
To: pgoswami@quickclic.net
CC: materials-welding@googlegroups.com

Dear sir,

   it will be for power plant, especially for facilities in front of water sea.


Regards.


2013/4/13 pgoswami <pgoswami@quickclic.net>
Where you want use these pipes?
 
Would it be for power plant application or for design and construction of any oil and gas plant ?
 
Please elaborate.
 
Thanks
 

Pradip Goswami,P.Eng.IWE

Welding & Metallurgical Specialist

Ontario, Canada.

Email-pgoswami@sympatico.ca,

pgoswami@quickclic.net

 


From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Zakaria ghrab
Sent: Friday, April 12, 2013 12:23 PM
To: materials-welding@googlegroups.com
Subject: [MW:17357] Austinitic Stainless steel piping, corrosion environnement


Dear experts,

  Need your help.

Need to confirm if we can use austinitic stainless steel piping (A312 304L & 316L grades)  for maritime environnent and any risk of corrosion.

To code/standard i can refer ?

Regards.

-----
زكرياء غراب
GHRAB Zakaria
Jorf Lasfar Units 5&6 Power Plant construction Project
EA2C/ SDEM Entreprises
Site QA/QC Manager
Mobile : Morocco (+212) 6 61 07 00 11
             Tunisia (+216) 96 635 805



Yesterday is the pass, tomorrow is the future; and today? Today is the present, the gift: Enjoy it!

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
 
 



--
زكرياء غراب
GHRAB Zakaria
Jorf Lasfar Units 5&6 Power Plant construction Project
EA2C/ SDEM Entreprises
Site QA/QC Manager
Mobile : Morocco (+212) 6 61 07 00 11
             Tunisia (+216) 96 635 805



Yesterday is the pass, tomorrow is the future; and today? Today is the present, the gift: Enjoy it!

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
 
 

No comments:

Re: [MW:34913] Filler wire

E71T-1C  is Charpy Impact tested at -20degC E71T-1CJ is Charpy impact tested at -40degC. AWS Classification for FCAW is only a supplementary...