unstamped vessel no AI is involved, this can be recertified
On Tue, Apr 16, 2013 at 1:30 PM, Mhaskar Aly <mhaskar.aly@gmail.com> wrote:
Dear friend,Thank you for your advise...Can following clause of SA20 will work...13.4 Subdivided Plates:
13.4.1
By agreement between the purchaser and the
manufacturer or processor, each subdivided plate (a plate
separated from a master plate) shall be legibly marked with
the name, brand, or trademark of the organization that
subdivided the plate plus a code traceable to the required
markings, provided that the information required in 13.1,
cross referenced to that code, is furnished with the plates.
ThanksAliOn Tue, Apr 16, 2013 at 10:47 AM, rudolf saldanha <rudolf_jude@yahoo.com> wrote:
--Hi,Not an expert at all but just my 2 cents.Sec II, SA 20 - 13 clearly states the required markings. The key words are "SHALL". If this job is for audit purpose, I will definitely not go for it. But if it is a regular production the AI's approval may be sought. Finally the onus is on the manufacturer as far as the integrity of the vessel is concerned.
From: Mhaskar Aly <mhaskar.aly@gmail.com>
To: materials-welding@googlegroups.com
Cc: ali.m@velath.com
Sent: Tuesday, 16 April 2013, 13:04
Subject: [MW:17424] SA516 Gr70 plates having different markings are acceptable for ASME ustamped Pressure Vessel
--Dear ExpertsWe wanted to use SA516 Gr70 plate from DANSTEEL (MTCs' are attached) where original marking on plate is as followsURLR EH36 S355K2+N CE; refer the attachment(SA516 65/70MTLTV is not punched on plate; but the marking on plate is traceable to given mtc…Mtc shows Specification as ASME SA516 65/70 LR EH36 S355K2+NMill has issued letter regarding modification of marking as ASME SA561 65/70 MT LTV…(refer attachment)We internally released these plates as marking on plate is traceable to MTC…further there is letter from Mill regarding the marking.Kindly advise can we use this plate for ASME U Stamped Pressure vessel jobAli
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
No comments:
Post a Comment