Re: [MW:17433] Requirements for Welding Electrode / Filler Wire

pl find attachment which may usefull to u

Pandithan
Welding Consultant


On Tue, Apr 16, 2013 at 2:44 PM, kannayeram gnanapandithan <kgpandithan@gmail.com> wrote:
what is test coupen thickness because preheat varies with thickness

Pandithan
Welding Consultant


On Sun, Apr 14, 2013 at 8:12 PM, v baskar <vrbaskar2007@gmail.com> wrote:

   Dear  Experts,


We have to establish newly below PQR's as per ASME Sec. IX.    Kindly suggest / advice the requirements of welding electrodes / filler wire, preheat /  inter-pass temperature and also provide if already established WPS / PQR's for my reference. 


              1.Material  HARDOX 500+HARDOX500 PROCESS : SMAW

             

              2.Material  HARDOX 500+HARDOX500 PROCESS : GMAW

 

              3.Material HARDOX500+ IS2062 Gr 'B' PROCESS: SMAW

 

              4.Material HARDOX500+ IS2062 Gr 'B' PROCESS: GMAW

 

              5.Material HARDOX500+SS304 PROCESS: SMAW



Best Regards


VB

    

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
 
 


--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
 
 

No comments:

[MW:34920] Tubesheet Hole step

Hello Team, I have one question any tolerance given for tubesheet Hole step. Please do needful. Regards, AP  -- https://materials-...