Austenitic SS 316 L is generally suitable in marine environment, but unsuitable for sour service conditions, specially when hydrogen sulphide gas is involved.



From: bruce alavi <alavib2001@yahoo.com>
To: "materials-welding@googlegroups.com" <materials-welding@googlegroups.com>; pgoswami <pgoswami@quickclic.net>
Sent: Monday, April 15, 2013 3:51 PM
Subject: Re: [MW:17388] Re: 17357] Austinitic Stainless steel piping, corrosion environnement

Suggest to coat the SS pipes to ensure longer corrosion protection, it is always a cost effective solution 
 
Very Best Regards
Behrooz Alavi

From: Zakaria ghrab <zakaria.ghrab@gmail.com>
To: pgoswami <pgoswami@quickclic.net>
Cc: "materials-welding@googlegroups.com" <materials-welding@googlegroups.com>
Sent: Saturday, April 13, 2013 10:12 AM
Subject: [MW:17368] Re: 17357] Austinitic Stainless steel piping, corrosion environnement

Dear sir,

   it will be for power plant, especially for facilities in front of water sea.


Regards.


2013/4/13 pgoswami <pgoswami@quickclic.net>
Where you want use these pipes?
 
Would it be for power plant application or for design and construction of any oil and gas plant ?
 
Please elaborate.
 
Thanks
 
Pradip Goswami,P.Eng.IWE
Welding & Metallurgical Specialist
Ontario, Canada.
 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Zakaria ghrab
Sent: Friday, April 12, 2013 12:23 PM
To: materials-welding@googlegroups.com
Subject: [MW:17357] Austinitic Stainless steel piping, corrosion environnement


Dear experts,

  Need your help.

Need to confirm if we can use austinitic stainless steel piping (A312 304L & 316L grades)  for maritime environnent and any risk of corrosion.

To code/standard i can refer ?

Regards.

-----
زكرياء غراب
GHRAB Zakaria
Jorf Lasfar Units 5&6 Power Plant construction Project
EA2C/ SDEM Entreprises
Site QA/QC Manager
Mobile : Morocco (+212) 6 61 07 00 11
             Tunisia (+216) 96 635 805



Yesterday is the pass, tomorrow is the future; and today? Today is the present, the gift: Enjoy it!
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to mailto:materials-welding%2Bunsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to mailto:materials-welding%2Bunsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
 
 



--
زكرياء غراب
GHRAB Zakaria
Jorf Lasfar Units 5&6 Power Plant construction Project
EA2C/ SDEM Entreprises
Site QA/QC Manager
Mobile : Morocco (+212) 6 61 07 00 11
             Tunisia (+216) 96 635 805



Yesterday is the pass, tomorrow is the future; and today? Today is the present, the gift: Enjoy it!
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
 
 


--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
 
 


No comments:

[MW:34866] Presentation for WPS ,PQR AND WPQ as per ASME Sec IX in power point

Dear Experts.        If anyone having presentation of WPS,PQR and WPQ  as per ASME  SEC.IX  in power point then please share . Regards Sanja...