Monday, April 15, 2013

Re: [MW:17410] WPS

Yes you can use Impact tested WPS/PQR for non-impact test requiring jobs.
 
Thanks & Regards

J.Gerald Jayakumar
00968-99438165
From: Ahmed Husain <ahmraha@yahoo.com>
To: "materials-welding@googlegroups.com" <materials-welding@googlegroups.com>
Sent: Sunday, April 14, 2013 9:43 PM
Subject: [MW:17393] WPS

Dear All,
 
Your valuable comment is required on following cases.
 
1. Suppose, if i have a certified PQR for P1 Gr1 to P1Gr1 material with PWHT and impact testing. Process is GTAW and SMAW. Based on this PQR, can I prepare a WPS without impact testing, i.e for materials and design condition doesn't require impact testing. There is no issue in other variables.
2. Is it acceptable to apply a 'WPS prepared and approved for low temperature service with impact testing ' to a job, for which there is no requirement for impact testing.
 
A. Husain
ABS Consulting Inc.
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
 
 


No comments:

[MW:34866] Presentation for WPS ,PQR AND WPQ as per ASME Sec IX in power point

Dear Experts.        If anyone having presentation of WPS,PQR and WPQ  as per ASME  SEC.IX  in power point then please share . Regards Sanja...