hi, the attached file was contributed by one of the members, Check it out.But am afraid, there is no reference to any code as such.
From: Yasir Bhatti <meloyasir2@gmail.com>
To: materials-welding@googlegroups.com
Sent: Saturday, 13 April 2013, 23:19
Subject: [MW:17365] Non Standard Blind Flange (Fabricated from Plate)
Dear Experts,
-- I am need of your help , i have got blind flange fabricated from plate selection chart from this forum but difficult to prove to client can you please give me code reference or derived formula.
Your Earliest Response is highly appreciated.
Thanks and Regards,
Yasir
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
No comments:
Post a Comment