Dear Mr. Pundir, I suggest you to keep holding period 30 Minutes considering 10 mm. Nom. Thk. Following vendors can do the job successfully. (1) Ratnamani Heating Point, Odhav, Ahmedabad- Contact No. 079-22974313. (2) Heat treaters & Engineers- Ankleshwar- Contact No. TELFAX NO 02646-221190. (3) Gujrat Perfect Engg. Ltd., Vadodara- 9898014997. Thanks & regards, C. R. GANDHI
--- On Fri, 4/12/13, A. K. Pundir <pundir@milindia.in> wrote:
From: A. K. Pundir <pundir@milindia.in> Subject: [MW:17353] Quenched annealing of SS 116 Vessel To: materials-welding@googlegroups.com Date: Friday, April 12, 2013, 11:31 AM
Dear All, Need your suggestions on PWHT(Quenched annealing) of SS 116 Vessel with following details. 1.T.L to T.L=1590mm 2.Totel length=2165mm 3.Shell Dia=1168mm 4.Thickness=10mm 5.Material A240 TP 316L,A312 TP 316,A182 TP 316. 6.Soaking Temperature-1950 ̊F 7.Soaking Time- 105 minutes 8.Rate of Cooling-water Quenching If this Heat Treatment is possible please suggest the good Heat Treatment shop in India. Regards A.K.Pundir Dy. Manager(Q.A) MILINDIA LTD., W-31, SECTOR-11, NOIDA - 201 301 (U.P) 09871607731 ** Message has been scanned by Emergic MailServ ** -- To post to this group, send email to materials-welding@googlegroups.com To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com For more options, visit this group's bolg at http://materials-welding.blogspot.com/ http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents. --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com. For more options, visit https://groups.google.com/groups/opt_out.
|
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at
http://materials-welding.blogspot.com/ http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit
https://groups.google.com/groups/opt_out.
No comments:
Post a Comment