Dear Friend 

First you need to give proper support in preassembly of Clenout door to resist  deformation which will come out during the Strees Relieving Process.
After  that u have to Select location of you couple  As per  API 650. 



On Wed, Apr 10, 2013 at 12:29 PM, george keribo <berepele@gmail.com> wrote:

I want to know if there is a different way to perform stress relieving on a tank cleanout flush opening assembly after is has been installed . Because according to API 650, stress relieve to be done on the preassembled cleanout fitting ..5.7.7.3 before installation. I need a suggestion on how to carry out the thermal stress relieve.

On Mar 16, 2013 12:18 PM, "george keribo" <berepele@gmail.com> wrote:

Thats my calculation also buh my coleague had a different consideration , he calculated it considering the shell thickness ... I got it ,, thnx

On Mar 16, 2013 9:18 AM, "Karthikeyan R" <rkarthikeyanapt@gmail.com> wrote:
HI,
 
The Plumbness depends upon the height from where you measure, you should not consider the thickness,
 
According To API 650 the Maximium out of Plumness should be 1/200
 
for your case you want to measure for the first course 2.5Mts (2500 mm)
 
so the calculation should be 1/200*(2500 mm)
 
i.e.,  ± 12.5mm ( The Shell course can lean inside or outside).
 
and the valuse you can measure ever 45° intevals (0°, 45°, 90° etc)
 
 
Regards
 
karthi


 
On Sat, Mar 16, 2013 at 12:15 AM, Jorge Mejía Lema <jmejialema@gmail.com> wrote:
I have very good experiance in tank construction: the pumbing tollerance should be cero (o.ooo) true vertical because this course is the reference base.
regards,
jml 


2013/3/15 george keribo <berepele@gmail.com>

Yes i know all of that but still need to know the acceptable criteria for 20mm thick shell plate with 2500mm height ... Im designing a tank of 33m diameter and 15m height. I want to take plumbness on the first course on 2.5m ....need to knw wat to have as out of plumbness acceptable criteria .

Thanks

On Mar 15, 2013 11:49 AM, "Usman Iqbal" <usman808@gmail.com> wrote:
ASTM A 6 acceptance criteria for flatness and waviness applies to each shell ring

Thanks
Usman

On Thu, Mar 14, 2013 at 9:17 PM, george keribo <berepele@gmail.com> wrote:

Plumbness and verticality check on tank first shell course . What is the calculation on how to check and the acceptable tolerance for each shell .

Thanks for your insights

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
 
 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
 
 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
 
 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
 
 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
 
 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
 
 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
 
 

No comments:

[MW:34866] Presentation for WPS ,PQR AND WPQ as per ASME Sec IX in power point

Dear Experts.        If anyone having presentation of WPS,PQR and WPQ  as per ASME  SEC.IX  in power point then please share . Regards Sanja...