FYI: The next edition of ASME Section IX will include fusion of HDPE.
John A. Henning
Welding & Materials
From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of manpreet
Sent: Tuesday, April 02, 2013 7:53 PM
To: materials-welding@googlegroups.com
Subject: Re: [MW:17277] HDPE Pipe INSTALLAITION ITP&WPS
Firdaus,
Refrain from commenting if you don't have the correct information, yes there are WPS for HDPE pipe.
Ramesh,
Inbox me a request and I will send you a copy.
Cheers
From: mohdfirdaus.abdrahim77@gmail.com
Sent: Tue, 02 Apr 2013 09:32:54
To: "materials-welding@googlegroups.com" <materials-welding@googlegroups.com>
Cc: "materials-welding@googlegroups.com" <materials-welding@googlegroups.com>
Subject: Re: [MW:17268] HDPE Pipe INSTALLAITION ITP&WPS
WPS?. I think there is no need for WPS. 2 type of fusion, electro fusion & butt fusion. It better you google it first before asking. Trust me, you'll find the solution when you google it. I found there too.
Mohd Firdaus Abd Rahim
QA/QC
+60122796361
Sent from my iPhone
On 02/04/2013, at 11:38 PG, Ramesh <ram2ram_2000@yahoo.com> wrote:
Dear all,
Any one can send HDPE PIPE under ground piping ITP &WPS FORMAT
Thanks
RAMESH
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
Get your own FREE website and domain with business email solutions, click here
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
______________________________________________________________________
The information in this email is confidential, and is intended solely for the addressee(s). If you are not the intended recipient of this email please let us know by reply and then delete it from your system; you should not copy this message or disclose its contents to anyone. The internet can not guarantee the integrity of this message. HAMON (and its subsidiaries) shall (will) not therefore be liable for the message if modified.
______________________________________________________________________
No comments:
Post a Comment