We had the FAT for valve already. But as I sent, in spec required we
have to seal test after weld valve to permanent pipe. That's the
difficulty I have. Many thanks.
On 4/2/13, Bui Son Truong <truongbs70@gmail.com> wrote:
> Dear Mr. Toan,
> Are you working in Vietnam, who is your client, consultant.
> Did they forget testing right after fabrication of spool ?
> Which function and pressure should be tested.
> Regularly you have to cut off pipe and install temporary spool (there are
> inlet, pressur gauge ...) for testing. And then replace by permanent pipe,
> welding joints should be ndt.
> How ever, this action should be follow project's procedure
> I will try find some document for your reference.
>
> Sent from my iPad
>
> On Apr 2, 2013, at 11:09 AM, Nguyễn Văn Toàn <toanvnguyen@ptsc.com.vn>
> wrote:
>
>> Dear Mr.Son,
>>
>> Yes, I'm Vietnamese and nice to see you :).
>> Thanks for your advice but what I need 's spec to refer and how to
>> check the valve seal leaking because the valve is installed in series.
>>
>> On 4/2/13, truong son bui <truongbs70@gmail.com> wrote:
>>> Dear Toan,
>>> Are you Vietnamese ? This is first time I see Vietnamese in this forum
>>> and
>>> is great.
>>> Your problem is simple: after welding, the welded valve may be
>>> inefficient
>>> by heating (shrink, crack ...) by slag. Those cause should make the
>>> valve
>>> be impaired.
>>> Inorder to sure it's functionality has been perfect, you should prepaire
>>> a
>>> temporary spool or hose and hydrolic pump ... for testing according by
>>> it's
>>> functionality. The testing proceduce should be approval by QA
>>> authorised.
>>> Wish success to you.
>>>
>>> On Mon, Apr 1, 2013 at 8:55 AM, toanvnguyen
>>> <nguyenvantoan221@gmail.com>wrote:
>>>
>>>> Dear Experts,
>>>>
>>>> We're doing a PLEM and TPAM project. The type of valves's welded-in
>>>> valve.
>>>> In spec. require as follow: "After fabrication's complete, welded-in
>>>> valves
>>>> shall be subject to seal tests in accordance with the relevant project
>>>> valve specification to demonstrate the valve functionality has not been
>>>> impaired during fabrication".
>>>> Could you pls give me some advice about this kind of tests. Many
>>>> thanks.
>>>>
>>>> --
>>>> To post to this group, send email to materials-welding@googlegroups.com
>>>> To unsubscribe from this group, send email to
>>>> materials-welding+unsubscribe@googlegroups.com
>>>> For more options, visit this group's bolg at
>>>> http://materials-welding.blogspot.com/
>>>>
>>>> http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
>>>>
>>>> The views expressed/exchnaged in this group are members personel views
>>>> and
>>>> meant for educational purposes only, Users must take their own
>>>> decisions
>>>> w.r.t. applicable code/standard/contract documents.
>>>> ---
>>>> You received this message because you are subscribed to the Google
>>>> Groups
>>>> "Materials & Welding" group.
>>>> To unsubscribe from this group and stop receiving emails from it, send
>>>> an
>>>> email to materials-welding+unsubscribe@googlegroups.com.
>>>> For more options, visit https://groups.google.com/groups/opt_out.
>>>>
>>>>
>>>>
>>>
>>>
>>>
>>> --
>>> Bui Son Truong - Director
>>> LILAMA Consultant Co.
>>> Address: 124 Minh Khai street, Hai Ba Trung Dist., Ha noi, Viet Nam.
>>> Fax: +84 3624 9416
>>> Tell: +84 3624 94 15
>>> Mobi:+84 9034 888 39
>>>
>>> --
>>> To post to this group, send email to materials-welding@googlegroups.com
>>> To unsubscribe from this group, send email to
>>> materials-welding+unsubscribe@googlegroups.com
>>> For more options, visit this group's bolg at
>>> http://materials-welding.blogspot.com/
>>> http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
>>>
>>> The views expressed/exchnaged in this group are members personel views
>>> and
>>> meant for educational purposes only, Users must take their own decisions
>>> w.r.t. applicable code/standard/contract documents.
>>> ---
>>> You received this message because you are subscribed to the Google
>>> Groups
>>> "Materials & Welding" group.
>>> To unsubscribe from this group and stop receiving emails from it, send
>>> an
>>> email to materials-welding+unsubscribe@googlegroups.com.
>>> For more options, visit https://groups.google.com/groups/opt_out.
>>>
>>>
>>>
>>
>>
>> --
>> Best Regards,
>> --------------------------------------------
>> Nguyen Van Toan
>> Piping & Machine Supervisor
>> Structure WS 2
>> - PTSC M&C
>> HP: 0907496198
>> email: toanvnguyen@ptsc.com.vn
>> Skype: toan_ptsc_mc
>>
>> --
>> To post to this group, send email to materials-welding@googlegroups.com
>> To unsubscribe from this group, send email to
>> materials-welding+unsubscribe@googlegroups.com
>> For more options, visit this group's bolg at
>> http://materials-welding.blogspot.com/
>> http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
>>
>> The views expressed/exchnaged in this group are members personel views and
>> meant for educational purposes only, Users must take their own decisions
>> w.r.t. applicable code/standard/contract documents.
>> ---
>> You received this message because you are subscribed to the Google Groups
>> "Materials & Welding" group.
>> To unsubscribe from this group and stop receiving emails from it, send an
>> email to materials-welding+unsubscribe@googlegroups.com.
>> For more options, visit https://groups.google.com/groups/opt_out.
>>
>>
>
> --
> To post to this group, send email to materials-welding@googlegroups.com
> To unsubscribe from this group, send email to
> materials-welding+unsubscribe@googlegroups.com
> For more options, visit this group's bolg at
> http://materials-welding.blogspot.com/
> http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
>
> The views expressed/exchnaged in this group are members personel views and
> meant for educational purposes only, Users must take their own decisions
> w.r.t. applicable code/standard/contract documents.
> ---
> You received this message because you are subscribed to the Google Groups
> "Materials & Welding" group.
> To unsubscribe from this group and stop receiving emails from it, send an
> email to materials-welding+unsubscribe@googlegroups.com.
> For more options, visit https://groups.google.com/groups/opt_out.
>
>
>
--
Best Regards,
--------------------------------------------
Nguyen Van Toan
Piping & Machine Supervisor
Structure WS 2
- PTSC M&C
HP: 0907496198
email: toanvnguyen@ptsc.com.vn
Skype: toan_ptsc_mc
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
Subscribe to:
Post Comments (Atom)
[MW:34916] Applicability of Impact requirement as per ASME B31.3
Dear All, Design code – ASME B31.3, Welding Code- ASME BPVC SEC IX Material to be used used during Fabrication - SA 333Gr6 (P No.1 G...
-
Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? ...
-
Definition of buttering from ASME Section IX, QW/QB-492 Definitions: Buttering: the addition of material, by welding, on one or bot...
-
Section I. PRINT READING 3-1. GENERAL a. Drawings . Drawing or sketching is a universal language used to convey all necessary information to...
No comments:
Post a Comment