Re: [MW:17263] Test subsea welded-in valve seal

Dear Toan,
Are you Vietnamese ? This is first time I see Vietnamese in this forum and is great.
Your problem is simple: after welding, the welded valve may be inefficient by heating (shrink, crack ...) by slag. Those cause should make the valve be impaired.
Inorder to sure it's functionality has been perfect, you should prepaire a temporary spool or hose and hydrolic pump ... for testing according by it's functionality. The testing proceduce should be approval by QA authorised.
Wish success to you.

On Mon, Apr 1, 2013 at 8:55 AM, toanvnguyen <nguyenvantoan221@gmail.com> wrote:
Dear Experts,

We're doing a PLEM and TPAM project. The type of valves's welded-in valve. In spec. require as follow: "After fabrication's complete, welded-in valves shall be subject to seal tests in accordance with the relevant project valve specification to demonstrate the valve functionality has not been impaired during fabrication".
Could you pls give me some advice about this kind of tests. Many thanks.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
 
 



--
Bui Son Truong - Director
LILAMA Consultant Co.
Address: 124 Minh Khai street, Hai Ba Trung Dist., Ha noi, Viet Nam.
Fax:  +84 3624 9416
Tell:  +84 3624 94 15
Mobi:+84 9034 888 39

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
 
 

No comments:

[MW:34916] Applicability of Impact requirement as per ASME B31.3

Dear All, Design code – ASME B31.3, Welding Code- ASME BPVC SEC IX Material  to be used used during Fabrication - SA 333Gr6 (P No.1 G...