Dear Friends We have PQR with F7A8 EM12K from ESAB Brand ; Can we use F7A8 EM12K from other Brands viz Bohler, Lincoln, Kiswel etc... Is it acceptable as per SEC IX... Ali Mhaskar | ||
|