Dear Expert,
Could you please give your opinion for following matter?
Combined welding process: GTAW + SAW
Test coupon: Single U
Plate thickness: 20 mm
GTAW - root pass and hot pass (approx. 4 or 5 mm)
SAW - filler pass and capping (approx. 16 mm)
Root to be back gouging and filled with SAW.
Question:
1. Does this welder / welding operator qualify to weld with GTAW and SAW? Root to be back gouging and filled with SAW.
2. Is separate qualification required to qualified this welder / welding operator for GTAW + SAW?
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
Subscribe to:
Post Comments (Atom)
Re: [MW:34832] Inquiry about Single Bevel with Back Grinding
Dear Uday, As per your question that one is called with backing only,Simple both side you are welding it is backing with strip or without st...
-
Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? ...
-
Definition of buttering from ASME Section IX, QW/QB-492 Definitions: Buttering: the addition of material, by welding, on one or bot...
-