Dear sir,

 

We are preparing an MDR.

 

Generally we are prepare MDR with the following points

1.material grade

2.if any material unique identification

3.heat number

4.item belongs to material grade (number of piece cut from plate)

5.UT report identification & traceability.

6.if any shipment details with unique number which will give summary for delivery.

 

Also sometimes we has to considered an if aay requirnments from client to be added & as well project specification.

 

Regards

 

Dinesh

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Maput Gani
Sent: Sunday, April 21, 2013 6:51 AM
To: materials-welding@googlegroups.com
Subject: [MW:17488] how to make material data report (MDR)

 

Dear Expert,

wondering, how to make material data report (mdr), or any one could share to me example mdr templates, procedure etc?



thanks in advanced

machfud

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
 
 

No comments:

[MW:34916] Applicability of Impact requirement as per ASME B31.3

Dear All, Design code – ASME B31.3, Welding Code- ASME BPVC SEC IX Material  to be used used during Fabrication - SA 333Gr6 (P No.1 G...