Hemant,
SB -729 specification covers UNS N08020, UNS N08026, and UNS N08024 pipe and tube for general corrosive service.
Which grade would be welded with SA 312 TP 316L??
Thanks
Pradip Goswami,P.Eng.IWE
Welding & Metallurgical Specialist
From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of hemant
Sent: Saturday, April 06, 2013 4:11 AM
To: materials-welding@googlegroups.com
Subject: [MW:17297] SB-729 ALLOY-20 MATERIAL WELDING CONSUMABLE.
Dear All,
We r going to weld SB -729 Pipe to SA312 TP 316L Pipe.
We have to prepare new WPS . anybody can suggest me which filler wire we have to use for GTAW.
Pls reply ASAP.
Regards
Hemant H suthar
Asst. Manager QA/QC
Chemithon Engineers Pvt Ltd.
Khanvel-Kheradi Road. Silvassa, UT of DNH
Website: www.chemithon.co.in
Office Contact: 0260 2677889 / 2677036 , 37 Cell : 9712973092
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
No comments:
Post a Comment