[MW:17297] SB-729 ALLOY-20 MATERIAL WELDING CONSUMABLE.

Dear All,

We r going to weld SB -729 Pipe to SA312 TP 316L Pipe.

We have to prepare new WPS . anybody can suggest me which  filler wire we have to use  for GTAW.

 

Pls reply ASAP.

 

 

Regards

Hemant H suthar

Asst. Manager QA/QC

Chemithon Engineers Pvt Ltd.

Khanvel-Kheradi Road. Silvassa, UT of DNH

Website: www.chemithon.co.in

Office Contact: 0260 2677889 / 2677036 , 37 Cell : 9712973092

 

No comments:

Re: [MW:34913] Filler wire

E71T-1C  is Charpy Impact tested at -20degC E71T-1CJ is Charpy impact tested at -40degC. AWS Classification for FCAW is only a supplementary...