On Sat, 16 Apr 2011 20:25:07 +0530 wrote
>
ER 347 is compatible fillet metal for this grade
From:
materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On
Behalf Of Zakaria ghrab
Sent: Friday, April 15, 2011 3:10 PM
To: materials-welding@googlegroups.com
Subject: [MW:10683] stainless steel Grade 321H Weldability
Hi all,
In our project we have to weld Austenetic SS grade 321H full GTAW, we
used ER 308 gtaw rod filler metal, one collegue say that we must use ER 347. is
it true ? use ER 308 is not compatible with these grade ?
Please help me
Regards
--
>
To post to this group, send email to materials-welding@googlegroups.com
>
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
>
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
>
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
>
Thanks with Regards From
TUSHAR GOHIL
Mobile No: 9510918745 & 7204626800
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
No comments:
Post a Comment