Re: [MW:10867] ASME/ASTM equivalent of S355J2+N

It is NOT ASTM A36. A36 has specified tensile of 420 N/mm2.


On Tue, Apr 26, 2011 at 4:44 PM, SENTHILKUMAR SWAMINATHAN <skumarswami@yahoo.co.in> wrote:
Vikas,
Refer attached may help you. Hope it is A36 (ASTM)
 
Regards,
S.SENTHILKUMAR



From: Vikas Bhandari <vikas.bhandari349@gmail.com>Sent: Tue, 26 April, 2011 9:09:50 AM

Subject: [MW:10855] ASME/ASTM equivalent of S355J2+N

Dear All

What is the ASTM/ASME equivalent of structural material S355J2+N (minimum yield strength 355 MPa, Tensile 470 to 630 MPa, C: 0.20 max, Si: 0.55 max, Mn: 1.60 max , CE: 0.45 max). A link to reference document stating the same would be much appreciated.

Thanks & best regards
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.



--
Arunachalam.A,
Abu Dhabi Gas Industries Ltd,
P.O.Box # 50124
Abu Dhabi, UAE
Mobile : +971-50-5257122

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34866] Presentation for WPS ,PQR AND WPQ as per ASME Sec IX in power point

Dear Experts.        If anyone having presentation of WPS,PQR and WPQ  as per ASME  SEC.IX  in power point then please share . Regards Sanja...