RE: [MW:10866] Re : Blasting and Paint on Weldment

We are thermal spraying 85% zinc / 15% aluminum inside an ASME section VIII Div. 2 pressure vessel, do we need to conform to any ASME code to perform this work?

Also does anyone in this forum have any data on zinc compatibility with refrigerants such as R134a or any of the refrigerants?

Regards,

David Stevenson

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of mustaffi
Sent: Tuesday, April 26, 2011 4:44 AM
To: materials-welding@googlegroups.com
Subject: RE: [MW:10862] Re : Blasting and Paint on Weldment

 

I understood ,

 

Right now we’re facing the issue to convince the client’s since we apply TSA and Coat and Sealer ..

See references  UG 99 in ASME VII

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of tamer said
Sent: Tuesday, 26 April, 2011 4:27 PM
To: materials-welding@googlegroups.com
Subject: Re: [MW:10857] Re : Blasting and Paint on Weldment

 

For any painting activities, ASME code is not applicable, only painting cods are applicable, also specially for painting you have to go to client specification which will guide you what paint system you have to apply.

 

Best regards

 

Tamer Said

Inspection Engineer

CSWIP 3.1  - BGAS Gr. 2 Holder

--- On Tue, 4/26/11, mustaffi <mustaffi@dynac.com.my> wrote:


From: mustaffi <mustaffi@dynac.com.my>
Subject: [MW:10851] Re : Blasting and Paint on Weldment
To: materials-welding@googlegroups.com
Date: Tuesday, April 26, 2011, 6:44 AM

 

Dear All,

 

Did anyone of you can help me for any references in ASME Code to proceed works for  Blasting and Paint at weldment area ..

I will go through with Thermal Spray Coating on that area..

 

Regards

Mus

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34820] RE: 34813] Clarification in Rate of heating and cooling.

Hello,   Please see the response below.   Regards.   P. Goswami, P. Eng, IWE.   From: materials-welding@googlegroups.com <materials-weld...