Hi Azmi,
 
CA-Corrosion Allowance
 
You may refer the material spec. to get the CA.
 
Thanks & Regards,
 
K. Babu
 
----- Original Message -----
From: asad azmi
Sent: Tuesday, April 26, 2011 1:17 PM
Subject: Re: [MW:10852] acceptance standards for pittings for SA 516 GR 70 Plates

Dear mr. Babu,
 
construction code is ASME SEC VIII DIV 1.
 
Pittings were observed  on the plates during material receiving inspection.
 
pls inform me what is CA.
 
thanks and regards

On Tue, Apr 26, 2011 at 4:10 AM, Kathalingam Babu <kathalingam.qaqc@ppl.com.sg> wrote:
Hi Azad,
 
You can consider the CA, as allowable depth of pitting allowed for the respective grade.
 
What is the construction code ?
 
Thanks & Regards,
 
K. Babu
----- Original Message -----
From: asad azmi
Sent: Monday, April 25, 2011 8:06 PM
Subject: [MW:10842] acceptance standards for pittings for SA 516 GR 70 Plates

Dear All,
 
Greetings.
 
what is the acceptance standard for pittings on SA 516 GR 70 Plate.
 
I mean what is the depth and diameter allowed.
 
Thanks and Regards
 
Asad Azmi

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34919] Welder qualification certificate

Dear All     anyone can share a format for welder certificate and card format        Thanks & Best Regards Saleem manhappulath Mob:+9665...