Dear Rohtak
 
IRIS can be used on all the materials wherever Ultrasounds can travel, We do specialize in IRIS and have sucessfully inspected HDPE and cement lined pipes as well.
 
Regards
Mohd, Ilyas
Dacon inspection Services.

On Tue, Apr 19, 2011 at 7:54 PM, VIKAS THAKUR <vt410401@gmail.com> wrote:
Can IRIS be used for alloy steels also? If not why?

Vikas
Gammon India Limited,
Rohtak


On Tue, Apr 19, 2011 at 10:25 AM, S. Waheedullah Shah <waheedullah@fatima-group.com> wrote:

Dear Ilangkumaran,

IRIS stands for Internal rotary inspection system which is based on UT and is used for inspection of pipes and tubes CS and SS.

Best regards,

Syed Waheedullah Shah

Unit Manager Inspection

Pakarab Fertilizers

Multan

Tel. Office: +92-61-90613098

Mob.: +92-333-3829925

            +92-300-2221535

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of k.ilangkumaran ilangkumaran
Sent: Tuesday, April 19, 2011 9:21 AM
To: materials-welding@googlegroups.com
Subject: [MW:10731] IRIS inspection

 

Dear experts,

 

                What is IRIS? where does this used? What is the limitations? Is this applicable only to inspect in CS tubing of boilers or both CS & SS.

 

Thanks in advance.

 

Regards

Ilangkumaran

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.



--
Thanking You
With Best Regards
Mohammed Ilyas Mohiuddin

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34866] Presentation for WPS ,PQR AND WPQ as per ASME Sec IX in power point

Dear Experts.        If anyone having presentation of WPS,PQR and WPQ  as per ASME  SEC.IX  in power point then please share . Regards Sanja...