Hi Azad,
 
You can consider the CA, as allowable depth of pitting allowed for the respective grade.
 
What is the construction code ?
 
Thanks & Regards,
 
K. Babu
----- Original Message -----
From: asad azmi
Sent: Monday, April 25, 2011 8:06 PM
Subject: [MW:10842] acceptance standards for pittings for SA 516 GR 70 Plates

Dear All,
 
Greetings.
 
what is the acceptance standard for pittings on SA 516 GR 70 Plate.
 
I mean what is the depth and diameter allowed.
 
Thanks and Regards
 
Asad Azmi

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34916] Applicability of Impact requirement as per ASME B31.3

Dear All, Design code – ASME B31.3, Welding Code- ASME BPVC SEC IX Material  to be used used during Fabrication - SA 333Gr6 (P No.1 G...