Re: [MW:10795] Hardness of SA516 all grade

0.3*uts =bhn hardness

On 1/21/11, adwenda@gmail.com <adwenda@gmail.com> wrote:
> Dear experts,
>
> Please advise the hardness value of SA516 for all grade (with ref. detail)
> since it is not mentioned either in ASME sect. II/IX or the correspond ASTM.
>
> Even we can take the figure from conversion table or theoretical formula,
> I'm not confidence of using this as reference.
>
> Appreciate for your feedback on this
>
> Thanks and Rgds
> A.D. Wenda - Indonesia
>
> --
> To post to this group, send email to materials-welding@googlegroups.com
> To unsubscribe from this group, send email to
> materials-welding+unsubscribe@googlegroups.com
> For more options, visit this group's bolg at
> http://materials-welding.blogspot.com/
> The views expressed/exchnaged in this group are members personel views and
> meant for educational purposes only, Users must take their own decisions
> w.r.t. applicable code/standard/contract documents.
>

--
Sent from my mobile device

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34820] RE: 34813] Clarification in Rate of heating and cooling.

Hello,   Please see the response below.   Regards.   P. Goswami, P. Eng, IWE.   From: materials-welding@googlegroups.com <materials-weld...