Re: [MW:10793] Impact testing temp. for EN19 steel

Dear Sir,
            If the application is room temperature, the test temperature shall be 0°C; due to safety factors.
Regarding casting and plate, plate has better properties than casting as it is rolled and grains are more aligned with fine grain 7 to 8. In casting, if u can demonstrate a ASTM grain size of 5 or greater, u can very well use the casting tooooo.

2011/4/20 PREM SHANKARDUTT NAUTIYAL <prem_nautiyal@rediffmail.com>
Dear Friends

I wanted to use EN 19 plate in one of my present project, wherein the application demands severe impact loads at room temperature.

I had browsed through the properties of EN 19 plate in various literatures wherein the Izod test values are mentioned @ 55J.

However the Izod testing temperature is not mentioned.

Can anyone help me out or guide me where to refer, so that i can know the Izod testing temperature of this EN 19 steel.

Secondly i would also like to know which of the two will have more toughness and why - EN 19 casting OR EN19 plate ?
The reason being the final component will have to be casted due geometrical complications.


Regards

Prem Nautiyal


PREM S NAUTIYAL
CELL : 9769316004

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.



--
regards,
Harish.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34820] RE: 34813] Clarification in Rate of heating and cooling.

Hello,   Please see the response below.   Regards.   P. Goswami, P. Eng, IWE.   From: materials-welding@googlegroups.com <materials-weld...