Thursday, April 21, 2011

RE: [MW:10784] Repair Electrode for grey cast iron

Use Eutectic Xyron 223 with base of Eutectrode 27 or ESAB 92.58 
Rgds
Ajay goel


Date: Thu, 21 Apr 2011 12:21:58 +0400
Subject: [MW:10775] Repair Electrode for grey cast iron
From: sujay1199@gmail.com
To: materials-welding@googlegroups.com

Dear All,
 
can suggest me welding electrode for grey cast iron repair(ie porosity, blow holes)
 
regards

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.