Thursday, April 21, 2011

Re: [MW:10765] Impact testing temp. for EN19 steel

Hi
 
Izod will be done at Room temp.,  Unless  otherwise specifically mentioned by spec.
 
Thanks & Regards,
 
K. Babu
----- Original Message -----
Sent: Wednesday, April 20, 2011 11:21 PM
Subject: [MW:10758] Impact testing temp. for EN19 steel

Dear Friends

I wanted to use EN 19 plate in one of my present project, wherein the application demands severe impact loads at room temperature.

I had browsed through the properties of EN 19 plate in various literatures wherein the Izod test values are mentioned @ 55J.

However the Izod testing temperature is not mentioned.

Can anyone help me out or guide me where to refer, so that i can know the Izod testing temperature of this EN 19 steel.

Secondly i would also like to know which of the two will have more toughness and why - EN 19 casting OR EN19 plate ?
The reason being the final component will have to be casted due geometrical complications.


Regards

Prem Nautiyal


PREM S NAUTIYAL
CELL : 9769316004

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34916] Applicability of Impact requirement as per ASME B31.3

Dear All, Design code – ASME B31.3, Welding Code- ASME BPVC SEC IX Material  to be used used during Fabrication - SA 333Gr6 (P No.1 G...