Hi,
 
It was mentioned in Sec-II PART 'C' table-7 of SFA 5.1, please refer once again.
 
Please find attached the chemical compositions for your quick reference.
 
Cheers!
 
Raj
 

On Wed, Apr 20, 2011 at 4:53 PM, senins welo <senins054@gmail.com> wrote:
Dears sirs,
            For AWS A 5.1 E7018,The chemical composition  for C, P, S VALUES not specified in ASME SEC 2 ,PART C, WHAT IS THE VALUE? WHERE?

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34916] Applicability of Impact requirement as per ASME B31.3

Dear All, Design code – ASME B31.3, Welding Code- ASME BPVC SEC IX Material  to be used used during Fabrication - SA 333Gr6 (P No.1 G...