Can IRIS be used for alloy steels also? If not why?

Vikas
Gammon India Limited,
Rohtak

On Tue, Apr 19, 2011 at 10:25 AM, S. Waheedullah Shah <waheedullah@fatima-group.com> wrote:

Dear Ilangkumaran,

IRIS stands for Internal rotary inspection system which is based on UT and is used for inspection of pipes and tubes CS and SS.

Best regards,

Syed Waheedullah Shah

Unit Manager Inspection

Pakarab Fertilizers

Multan

Tel. Office: +92-61-90613098

Mob.: +92-333-3829925

            +92-300-2221535

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of k.ilangkumaran ilangkumaran
Sent: Tuesday, April 19, 2011 9:21 AM
To: materials-welding@googlegroups.com
Subject: [MW:10731] IRIS inspection

 

Dear experts,

 

                What is IRIS? where does this used? What is the limitations? Is this applicable only to inspect in CS tubing of boilers or both CS & SS.

 

Thanks in advance.

 

Regards

Ilangkumaran

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34919] Welder qualification certificate

Dear All     anyone can share a format for welder certificate and card format        Thanks & Best Regards Saleem manhappulath Mob:+9665...