Dear Mr Senthi, You are fabricating piping as per which code? I dont think any code accepts 34mm length incomplete penetration except API even then I would suggest you to convince your production people and get it repair done. Regards Ilangkumaran
--- On Mon, 4/18/11, SENTHIL P <senbe381@gmail.com> wrote:
From: SENTHIL P <senbe381@gmail.com> Subject: [MW:10723] visual test To: materials-welding@googlegroups.com Date: Monday, April 18, 2011, 6:05 PM
Dear sir, 6 " std pipe 7.11mm for normal and M fluid visually we find incomplete pentration 34mm in any 150mm ,depth 2mm in random manner, is it accepted? please explain and we find 1mm or small visually seen porosity on surface of weld ,is need to repair or not? we can grind this but prodution people not allowed, please explain thank u, senthil -- To post to this group, send email to materials-welding@googlegroups.com To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com For more options, visit this group's bolg at http://materials-welding.blogspot.com/The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
|
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at
http://materials-welding.blogspot.com/ The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.