Dear Vino,

Please have a look at Qw-420.2 which allows you to use ASTM material for qualification.

In 2009, changes were made and S no. was removed from ASME Sec ix, "Base materials previously assigned S no were reassigned the corresponding P no or P no plus Gr no"

ASTM material shall have same P no as assigned to ASME material (SA333 Gr6 - P1 Gr1 & A350 LF2 - P1 Gr2)

Regards
Manpreet Singh



On Tue, 19 Apr 2011 06:05:36 +0530 Vino Varghese <vinopvarghese@gmail.com> wrote
>
Dear All,
 
Design Code: ASME Sec VIII, Div 1
U-Stamp Pressure Vessel
 
Reference Code : ASME Sec IX, Edition 2007, Add 09
Material of Construction: SA 516 Gr 70N(30mm thk)
PQR Material : 1. Pipe - ASME SA 333 and 2. Flange : ASTM A350 LF2
 
Query:
Is it mandatory that Qualification has to be done only with a ASME Material?
If ASTM Material is used for qualification, then WPS will be qualified only for that particualr Material and cannot be Qualified as P1 Material. Please provide all reference from Code for justification.
 
Hope to see that i was able to communicate properly with regard to raised query.
 
Expecting as usual response from all sides.
 
Thanks & Regards
Vino-Doha
 
 
 
 
 

--
>To post to this group, send email to materials-welding@googlegroups.com
>To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
>For more options, visit this group's bolg at http://materials-welding.blogspot.com/
>The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
>

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34919] Welder qualification certificate

Dear All     anyone can share a format for welder certificate and card format        Thanks & Best Regards Saleem manhappulath Mob:+9665...