Re: [MW:10725] visual test

Dear Senthil

If your code is B31.3, please refer to table 341.3.2 to get the answer. Incomplete penetration and surface porosity are not acceptable (no imperfection).

rgds

2011/4/18 SENTHIL P <senbe381@gmail.com>
Dear sir,
      6 "  std pipe 7.11mm for normal and M fluid
visually we find incomplete pentration 34mm in any 150mm ,depth 2mm in random manner, is it accepted? please explain
 and we find 1mm or small visually seen porosity on surface of weld ,is need to repair or not? we can grind this but prodution  people not allowed, please explain
 thank u,
senthil

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:34913] Filler wire

E71T-1C  is Charpy Impact tested at -20degC E71T-1CJ is Charpy impact tested at -40degC. AWS Classification for FCAW is only a supplementary...