Re: [MW:10717] stainless steel Grade 321H Weldability

Hi,
Please refer Table 5 of ASTM A312-06. It is very clear.
Paulose John

On Sun, Apr 17, 2011 at 6:15 PM, kannayeram gnanapandithan <kgpandithan@gmail.com> wrote:
for Gtaw, either ER321 Or ER347 shall be used but for SMAW only E347 is to be used because if we use E321, there will be loss of Titanium alloying loss in arc stream
pandithan

On Fri, Apr 15, 2011 at 3:10 PM, Zakaria ghrab <zakaria.ghrab@gmail.com> wrote:
Hi all,

  In our project we have to weld Austenetic SS grade 321H full GTAW, we used ER 308 gtaw rod filler metal, one collegue say that we must use ER 347. is it true ? use ER 308 is not compatible with these grade ?

Please help me


Regards

--

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34916] Applicability of Impact requirement as per ASME B31.3

Dear All, Design code – ASME B31.3, Welding Code- ASME BPVC SEC IX Material  to be used used during Fabrication - SA 333Gr6 (P No.1 G...