Hi,
The minimum tensile strength requirement either by ASME Sec-IX or API 1104 is the "minimum base material strength". In this case the minimum base material strength required for API 5L X65 is "77000 Psi or 530 Mpa". If you weld with E7016-1 & E7018-1 you will get only 70,000 Psi maximum as these electrodes are designed for a maxi of 70,000 PSi.
You have to choose, suitable consumable i.e 8018-G etc. (Refer A5.5)
Hope this will clarify.
Cheers!
Raj
On Sun, Apr 17, 2011 at 1:41 PM, VENKATA SWAMI REDDY KARRI <kvsreddy777@gmail.com> wrote:
Minimum Tensile requirements is 77600 psi ,if the specimen breaks in the weld or fusion zone and the observed strength equal to 77600 psi or greater than it acceptable according to API 1104 5.6.2.3.But check your project specification.
On Sun, Apr 17, 2011 at 10:10 AM, zaheer abbas <zaheer.spsl@yahoo.com> wrote:
--Dear Allwe welded to establish a procedure API 5LX65 thickness 16mm material with E7016-1 and E7018-1 esab low hydrogen electrode.some of my frient told me it is difficult to pass tensile test requirements of API 5LX65 and coupon sample may brack in weld metal.Please guide me if you experienced this type of failure and if the coupon bracks in weld metal what value of tensile strength is acceptable?Best RegardsZaheer
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
No comments:
Post a Comment