Yes this is correct but if governing thickness code is ASME B 31.3. Otherwise qualification range will be 8 to 16 mm according to ASME 9.
Regards,
NAJM UL ISLAM
Welding Engineer
Velosi Certification Qatar
+974 6664 5393
From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of saji jos
Sent: Sunday, April 17, 2011 10:09 AM
To: materials-welding@googlegroups.com
Cc: raja sekhar; Ali Asghari
Subject: Re: [MW:10696] qualified thickness range
With impact test thickness range is t/2 to t+6 means (8/2mm =4mm ) to (8+6=14mm)
Means with Impact test thk range is 4m to 14mm
Without impact test thk range is 4.8mm to 16mm is currect
Saji Jos P
AbuDhabi
00971 56 6742779
From: raja sekhar <raj.inspection@gmail.com>
To: materials-welding@googlegroups.com
Sent: Sun, 17 April, 2011 8:01:07 AM
Subject: Re: [MW:10693] qualified thickness range
Yes,
I think you are refring to same supporting PQR only for the both thickness ranges.
For E.g, If you have qualified a PQR with a thk of 8 mm with impact test.
Your qualification ranges in the WPS will be
8 to 16 mm (WIth Impact test)
5 to 16 mm (Without Impact test)
You can write both the reading in the WPS.
Hope this will clarify.
Cheers!
Raj
On Thu, Apr 14, 2011 at 7:57 AM, Ali Asghari <asghariali@rocketmail.com> wrote:
Dear all
Is it possible a WPS issued that have two qualified thickness ranges?( one of them supported by a PQR that impact tested and another range with ignorance of the CVN results acc to ASME IX)
Regards.
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
No comments:
Post a Comment